Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | >= 500 °C | >= 932 °F | via DSC |
Specialty Coating Systems Parylene HT® Poly (P-Xylylene) Coating Parylene HT is a polymer of para-xylylene with the alpha hydrogen atoms of the N dimer replaced with fluorine. This variant of Parylene is useful in high temperature applications (short term up to 4.. |
|||
Melting Point | 500 °C | 932 °F | |
Goodfellow Zinc 95/Copper 5 Alloy Information provided by Goodfellow. |