Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 280 - 335 °C | 536 - 635 °F | Average value: 303 °C Grade Count:8 |
Overview of materials for Liquid Crystal Polymer (LCP), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 20% Glass Fiber Filled". Specific grades with glass content between 15% an.. |
|||
Melting Point | 280 - 335 °C | 536 - 635 °F | Average value: 314 °C Grade Count:20 |
Overview of materials for Liquid Crystal Polymer (LCP), Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), Mineral Filled". Each property range of values reported is minimum and max.. |
|||
Melting Point | 325 - 335 °C | 617 - 635 °F | |
Isoflon Virgin PTFE Polytetrafluoroethylene Properties/Improved compression and wear resistanceExcellent chemical stabilityBetter thermal conductivityExcellent resistance to continuous service temperatures up to 260°C, and, for limited per.. |
|||
Melting Point | 325 - 335 °C | 617 - 635 °F | ASTM D3418 |
Solvay Specialty Polymers Algoflon® L101 Polytetrafluoroethylene (PTFE) Algoflon® L101 a white PTFE micronized powder produced from dispersion polymerization comprising loose agglomerates of sub-micron sized primary particles. Algoflon® L101 can be de-agglomerated.. |
|||
Melting Point | 325 - 335 °C | 617 - 635 °F | ASTM D3418 |
Solvay Specialty Polymers Algoflon® L203F Polytetrafluoroethylene (PTFE) Algoflon® L203F a white PTFE micronized powder produced from dispersion polymerization comprising loose agglomerates of sub-micron sized primary particles. Algoflon® L203F can be de-agglomerat.. |
|||
Melting Point | 325 - 335 °C | 617 - 635 °F | ASTM D3418 |
Solvay Specialty Polymers Algoflon® L206 Polytetrafluoroethylene (PTFE) Algoflon® L206 a white PTFE micronized powder produced from dispersion polymerization comprising loose agglomerates of sub-micron sized primary particles. Algoflon® L206 can be de-agglomerated.. |
|||
Melting Point | 325 - 335 °C | 617 - 635 °F | ASTM D3418 |
Solvay Specialty Polymers Algoflon® L206F Polytetrafluoroethylene (PTFE) Algoflon® L206F a white PTFE micronized powder produced from dispersion polymerization comprising loose agglomerates of sub-micron sized primary particles. Algoflon® L206F can be de-agglomerat.. |
|||
Melting Point | 325 - 335 °C | 617 - 635 °F | ASTM D3418 |
Solvay Specialty Polymers Algoflon® L203 Polytetrafluoroethylene (PTFE) Algoflon® L203 a white PTFE micronized powder produced from dispersion polymerization comprising loose agglomerates of sub-micron sized primary particles. Algoflon® L203 can be de-agglomerated.. |