Thermal Properties Metric English Comments
Melting Point 657.2 - 688 °C
1215 - 1270 °F
Lucas-Milhaupt FOS FLO 670 Copper Phosphorus Tin Braze Filler Metal
Applications:Fos-Flo 7 iFos-Flo 670 is a low cost brazing filler metal suitable for joining copper to copper and copper to copper alloys where critical impact or vibration stresses are not encounter..