Material Notes:
Applications:Fos-Flo 7 iFos-Flo 670 is a low cost brazing filler metal suitable for joining copper to copper and copper to copper alloys where critical impact or vibration stresses are not encountered in service. It should only be used on assemblies where good fitup can be maintained. Characteristics: Fos-Flo 670 is a copper rich, low temperature, brazing filler metal that is free flowing and self-fluxing on copper by virtue of its phosphorus content. This alloy is extremely fluid when heated rapidly to its flow point and will penetrate joints with very little clearance. Best results are obtained with joint clearances of .001-.003 in. (.025 mm - .075 mm). The self-fluxing property of Flo 670 is effective on copper only. Copper base alloys, such as brass or bronze, may be brazed with Fos Flo 670 if the joints are coated with Handy Flux. Fos Flo 670 should not be used on ferrous metals or nickel base alloys, since the phosphorus produces brittle iron or nickel phosphides at the joint interface. Information provided by Lucas-Milhaupt, Inc.
Thermal Properties Metric English Comments
Melting Point 657.2 - 688 °C
1215 - 1270 °F
Solidus 657.2 °C
1215 °F
Melting Point
Liquidus 688 °C
1270 °F
Flow Point
Component Elements Properties Metric English Comments
Copper, Cu >= 86.25 %
>= 86.25 %
Other, total <= 0.15 %
<= 0.15 %
Phosphorous, P 6.0 - 6.4 %
6.0 - 6.4 %
Tin, Sn 6.7 - 7.2 %
6.7 - 7.2 %
Processing Properties Metric English Comments
Processing Temperature 688 - 788 °C
1270 - 1450 °F
Brazing Range
Descriptive Properties Value Comments
Color Light Brown