Thermal Properties Metric English Comments
Melting Point 76.0 °C
169 °F
Exxon Method
ExxonMobil Escor® AT-320 EMAAA Terpolymer for Polymer Modification  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.45 Acid Number. Provides unusual adhesion to a variety of substrates and other components, such as aluminum foil, polyolefins, polycarbonate, PET, ..
Melting Point 76.0 °C
169 °F
Freezing Point via DSC/ASTM D3418
DuPont Bynel® 1E554 Modified EVA Adhesive Resin  (discontinued **)
Bynel® Series 1100 resins are modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylen..
Melting Point 76.0 - 89.0 °C
169 - 192 °F
Solvay RHODAFAC® ASI-100 Octyl phosphonic acid
Identification: ALKYL PHOSPHONATE DERIVATIVECAS: 4724 – 48 – 5EINECS: 225 – 218 – 5Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: Corrosion inhi..
Melting Point 76.0 °C
169 °F
Freezing Point; ASTM D3417
DuPont Elvax® 3134SBZ Ethylene Vinyl Acetate
DuPont™ Elvax® 3134SBZ is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins. Additiv..
Melting Point 76.0 °C
169 °F
Freezing Point; ASTM D3418
DuPont™ Bynel® 21E810 Anhydride Modified Ethylene Acrylate
BYNEL® Series 2100 resins are anhydride modified ethylene acrylate resins. They contain a temperature stable ester that allows them to be functional in high temperature coextrusions. They are avail..
Melting Point 76.0 °C
169 °F
DSC
Arkema Group EVATANE® 28-03 Copolymer Ethylene - Vinyl Acetate
EVATANE® 28-03 is a random copolymer of Ethylene and Vinyl Acetate made by high-pressure radicalar polymerisation process. EVATANE® 28-03 is stabilized with antioxidants. The High Vinyl Acetate co..
Melting Point 76.0 °C
169 °F
Freezing Point; ASTM D3417, ISO 3146
DuPont™ Surlyn® 1825 Zinc Ionomer
Surlyn® 1825 is available for use in conventional blown, cast film, sheet extrusion and coextrusion equipment designed to process polyethylene and ethylene copolymer type resins. SURLYN® 1825 comp..
Melting Point 76.0 °C
169 °F
Freezing Point via DSC/ASTM D3418
DuPont Elvax® 3130SB Ethylene-Vinyl Acetate Copolymer Resin for Blown Film  (discontinued **)
12 wt% Vinyl Acetate.General Elvax® information: Elvax® packaging grade resins include low seal temperatures for use in coextrusions or for packaging temperature sensitive materials, excellent dra..
Melting Point 76.0 °C
169 °F
Freezing Point via DSC/ASTM D3418
DuPont Elvax® 3130SBZ Ethylene-Vinyl Acetate Copolymer Resin for Blown Film  (discontinued **)
12 wt% Vinyl Acetate.General Elvax® information: Elvax® packaging grade resins include low seal temperatures for use in coextrusions or for packaging temperature sensitive materials, excellent dra..
Melting Point 76.0 °C
169 °F
Freezing Point via DSC/ASTM D3418
DuPont Elvax® 3134Q Ethylene-Vinyl Acetate Copolymer Resin for Extrusion Coating, Casting  (discontinued **)&l
12 wt% Vinyl Acetate.General Elvax® information: Elvax® packaging grade resins include low seal temperatures for use in coextrusions or for packaging temperature sensitive materials, excellent dra..
Melting Point 76.0 °C
169 °F
Freezing Point via DSC/ASTM D3418
DuPont Nucrel® 1207 Ethylene-Methacrylic Acid Copolymer Resin for Extrusion Coating/Laminating  (discontinued
12 wt% Methacrylic Acid.Nucrel® 1207 is an ethylene-methacrylic acid copolymer resin available for use in conventional extrusion coating, coextrusion coating, and extrusion laminating equipment des..