Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 966 - 1040 °C | 1770 - 1900 °F | |
Universal Wire Works BNi-2 (AMS 4777) Nickel Base Brazing Filler Metal Information provided by Universal Wire Works for their line of welding wire and filler metal. |
|||
Melting Point | 966 - 1024 °C | 1770 - 1875 °F | |
Universal Wire Works BNi-3 (AMS 4778) Nickel Base Brazing Filler Metal Information provided by Universal Wire Works for their line of welding wire and filler metal. |
|||
Melting Point | 966 °C | 1770 °F | |
Goodfellow Nickel 62/Silicon 38 Alloy Information provided by Goodfellow. |