Thermal Properties Metric English Comments
Dropping Point 190 °C
374 °F
ASTM D2265
ExxonMobil 0 Mobilux EP
Mobilux EP 0, 1, 2, 3, and 023 products are a high performance family of five general-purpose industrial greases and two special-duty semi-fluid greases. These lithium hydroxystearate greases are fo..
Dropping Point 190 °C
374 °F
ASTM D2265
ExxonMobil 1 Mobilux EP
Mobilux EP 0, 1, 2, 3, and 023 products are a high performance family of five general-purpose industrial greases and two special-duty semi-fluid greases. These lithium hydroxystearate greases are fo..
Dropping Point 190 °C
374 °F
ASTM D2265
ExxonMobil 3 Mobilux EP
Mobilux EP 0, 1, 2, 3, and 023 products are a high performance family of five general-purpose industrial greases and two special-duty semi-fluid greases. These lithium hydroxystearate greases are fo..
Dropping Point 190 °C
374 °F
ASTM D2265
ExxonMobil 2 Mobilux EP
Mobilux EP 0, 1, 2, 3, and 023 products are a high performance family of five general-purpose industrial greases and two special-duty semi-fluid greases. These lithium hydroxystearate greases are fo..
Dropping Point 190 °C
374 °F
Dow Corning MOLYKOTE® G 68
Semi-synthetic greaseInformation provided by Dow Corning
Dropping Point >= 190 °C
>= 374 °F
Dow Corning MOLYKOTE® G-2001
Lithium thickened bearing grease based on synthetic hydrocarbonInformation provided by Dow Corning
Dropping Point 190 °C
374 °F
Dow Corning MOLYKOTE® LONGTERM 00 GREASE
NLGI 00 mineral oil greaseInformation provided by Dow Corning
Dropping Point >= 190 °C
>= 374 °F
Dow Corning MOLYKOTE® PG-75 GREASE
Semi-Synthetic (Mineral/PAO) grease especially for vehicle track-rod jointsInformation provided by Dow Corning
Dropping Point 190 °C
374 °F
ChevronTexaco Block Grease
Chevron Block Grease is a high melting point block grease.It is manufactured using highly refined base oils, a lithium thickener, and a special oxidation inhibitor which eliminates glazing and charr..
Dropping Point 190 °C
374 °F
ChevronTexaco NLGI 2 Ultra Duty Grease EP
FeaturesChevron Ultra-Duty Greases EP are versatile, multipurpose extreme pressure greases with high adhesive propertues designed for a wide variety of automotive and industrial applications.They ar..
Dropping Point 190 °C
374 °F
ASTM D2265
ExxonMobil 0 Mobilux EP
Mobilux EP 0, 1, 2, 3, and 023 products are a high performance family of five general-purpose industrial greases and two special-duty semi-fluid greases. These lithium hydroxystearate greases are fo..
Dropping Point 190 °C
374 °F
ASTM D2265
ExxonMobil 1 Mobilux EP
Mobilux EP 0, 1, 2, 3, and 023 products are a high performance family of five general-purpose industrial greases and two special-duty semi-fluid greases. These lithium hydroxystearate greases are fo..
Dropping Point 190 °C
374 °F
ASTM D2265
ExxonMobil 2 Mobilux EP
Mobilux EP 0, 1, 2, 3, and 023 products are a high performance family of five general-purpose industrial greases and two special-duty semi-fluid greases. These lithium hydroxystearate greases are fo..
Dropping Point 190 °C
374 °F
ASTM D2265
ExxonMobil 3 Mobilux EP
Mobilux EP 0, 1, 2, 3, and 023 products are a high performance family of five general-purpose industrial greases and two special-duty semi-fluid greases. These lithium hydroxystearate greases are fo..