Polymer Property : Dropping Point = 390 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Dropping Point 199 °C
390 °F
ASTM Test
Lubriplate 630-A Lithium Based Multi-Purpose Grease
These popular lithium type greases are excellent for a wide range of lubrication demands thus reducing the need to carry large grease inventories. They show exceptional resistance to water, steam, a..
Dropping Point 199 °C
390 °F
ASTM Test
Lubriplate EMB Lithium-Polymer Type Grease For Special Applications / Conditions
Lithium polymer type grease developed specifically for the lubrication of electric motor bearings, fans, and other high speed grease type ball and roller bearings. Applications: Electric motor beari..
Dropping Point 199 °C
390 °F
ASTM D566
Chesterton 613 Moly Grease
Description: Chesterton® 613 Moly Grease is a high-performance, cost-effective lubricant that can withstand extreme temperatures and pressures for a wide range of high and low-speed applications. F..
Dropping Point 199 °C
390 °F
ELM® TempFlex™ 35 to 160 Biodegradable Rail Curve Lubricant
Description: TempFlex™ 35 to 160 is a premium quality biodegradable, Biotechbased™ Rail Curve Lubricant formulated from USA-grown vegetable oils and a lithiumbased thickener.Applications: Designed..
Dropping Point 199 °C
390 °F
ELM® TempFlex™ 35 to 160 w/ MoS2 Biodegradable Rail Curve Lubricant
Description: TempFlex™ 35 to 160 now with molybdenum disulphide is a premium quality biodegradable, Biotechbased™ Rail Curve Lubricant formulated from USA grown vegetable oils and a lithium-based ..