Thermal Properties Metric English Comments
Specific Heat Capacity 0.840 - 0.880 J/g-°C
0.201 - 0.210 BTU/lb-°F
PEAK Werkstoff DISPAL S263 Aluminum Alloy, AlSi25Cu3Fe3Ni3MgCoTi, Condition T6
Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational..
Specific Heat Capacity 0.840 - 0.880 J/g-°C
0.201 - 0.210 BTU/lb-°F
PEAK Werkstoff DISPAL S263 Aluminum Alloy, AlSi25Cu3Fe3Ni3MgCoTi, Condition F
Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational..
Specific Heat Capacity 0.840 - 0.880 J/g-°C
0.201 - 0.210 BTU/lb-°F
PEAK Werkstoff DISPAL S263 Aluminum Alloy, AlSi25Cu3Fe3Ni3MgCoTi, Condition T4
Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational..
Specific Heat Capacity 0.840 J/g-°C
0.201 BTU/lb-°F
Microtherm Group MT Thermosphere® Moldable Insulation Paste
MT Thermosphere® is a low density temperature resistant paste with excellent thermal insulation properties from cryogenic to high temperature exposure. It is a perfectly seamless insulation syste..
Specific Heat Capacity 0.840 J/g-°C
0.201 BTU/lb-°F
Schott N-BAF51 Glass
Information Provided by SCHOTT North America, Inc.
Specific Heat Capacity 0.840 J/g-°C
0.201 BTU/lb-°F
Skamol Group SUPER 1100 E Calcium Silicate Insulating Slab
SKAMOL SUPER calcium silicate slabs have the following characteristics: Max. service temperature: Up to 1100°C (2012°F)Back-up insulation onlyExtremely lightweightVery low thermal conductivity..
Specific Heat Capacity 0.840 J/g-°C
0.201 BTU/lb-°F
Skamol Group SUPER 1100 ET Calcium Silicate Insulating Slab
SKAMOL SUPER calcium silicate slabs have the following characteristics: Max. service temperature: Up to 1100°C (2012°F)Back-up insulation onlyExtremely lightweightVery low thermal conductivity..
Specific Heat Capacity 0.840 J/g-°C
0.201 BTU/lb-°F
Skamol Group SUPER ISOL Calcium Silicate Insulating Slab
SKAMOL SUPER calcium silicate slabs have the following characteristics: Max. service temperature: Up to 1100°C (2012°F)Back-up insulation onlyExtremely lightweightVery low thermal conductivity..
Specific Heat Capacity 0.840 J/g-°C
0.201 BTU/lb-°F
DSC
Wolf Kunststoff ZEDEX® ZX-530EL3 066 Polymer Alloy, Carbon Fiber Reinforced
Main Characteristics: Low thermal expansion; High rigidity; High yield stress; High wear resistance; Low friction; Stress ResistantApplications: Chemical Engineering; Laboratory Technology; Automitv..