Thermal Properties Metric English Comments
Specific Heat Capacity 0.251 J/g-°C

@Temperature 20.0 °C
0.0600 BTU/lb-°F

@Temperature 68.0 °F
Hogen Duralloy H1W 55 Tungsten/45 Copper PM Metal Composite
RWMA Class 10.Hogen Duralloy refractory alloys are manufactured by pressing, sintering, and infiltrating tungsten with copper or silver.Typical Resistance Welding Applications: Class 10 material is ..