Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.373 J/g-°C | 0.0891 BTU/lb-°F | RT |
Haynes Hastelloy® B-3® alloy, 0% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Specific Heat Capacity | 0.373 J/g-°C | 0.0891 BTU/lb-°F | RT |
Haynes Hastelloy® B-3® alloy, 10% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Specific Heat Capacity | 0.373 J/g-°C | 0.0891 BTU/lb-°F | RT |
Haynes Hastelloy® B-3® alloy, 20% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Specific Heat Capacity | 0.373 J/g-°C | 0.0891 BTU/lb-°F | RT |
Haynes Hastelloy® B-3® alloy, 3.2 mm bright annealed sheet The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Specific Heat Capacity | 0.373 J/g-°C | 0.0891 BTU/lb-°F | RT |
Haynes Hastelloy® B-3® alloy, 30% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Specific Heat Capacity | 0.373 J/g-°C | 0.0891 BTU/lb-°F | RT |
Haynes Hastelloy® B-3® alloy, 40% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Specific Heat Capacity | 0.373 J/g-°C | 0.0891 BTU/lb-°F | RT |
Haynes Hastelloy® B-3® alloy, 50% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Specific Heat Capacity | 0.373 J/g-°C | 0.0891 BTU/lb-°F | RT |
Haynes Hastelloy® B-3® alloy, 6.3 mm plate The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Specific Heat Capacity | 0.373 J/g-°C | 0.0891 BTU/lb-°F | |
Special Metals INCONEL® 686 Nickel Superalloy (UNS N06686) Plate 0.250 in (6.4 mm) Tensile strength (ultimate and yield) and elongation values reported here are typical for 0.250 inch plate. Other property values are typical of INCONEL® alloy 686.Data provided by the manufactu.. |
|||
Specific Heat Capacity | 0.373 J/g-°C | 0.0891 BTU/lb-°F | |
Special Metals INCONEL® 686 Nickel Superalloy (UNS N06686) Plate 0.500 in (12.7 mm) Tensile strength (ultimate and yield) and elongation values reported here are typical for 0.500 inch plate. Other property values are typical of INCONEL® alloy 686.Data provided by the manufactu.. |
|||
Specific Heat Capacity | 0.373 J/g-°C | 0.0891 BTU/lb-°F | |
Special Metals INCONEL® 686 Nickel Superalloy (UNS N06686) Round 1.500 in (38.1 mm) Tensile strength (ultimate and yield) and elongation values reported here are typical for 1.500 inch round. Other property values are typical of INCONEL® alloy 686.Data provided by the manufactu.. |
|||
Specific Heat Capacity | 0.373 J/g-°C | 0.0891 BTU/lb-°F | |
Special Metals INCONEL® 686 Nickel Superalloy (UNS N06686) Sheet 0.062 in (1.6 mm) Tensile strength (ultimate and yield) and elongation values reported here are typical for 0.062 inch sheet. Other property values are typical of INCONEL® alloy 686.Data provided by the manufactu.. |
|||
Specific Heat Capacity | 0.373 J/g-°C | 0.0891 BTU/lb-°F | RT |
Haynes Hastelloy® B-3® alloy, heat treated at 1065°C, rapid quenched The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ea.. |
|||
Specific Heat Capacity | 0.373 J/g-°C | 0.0891 BTU/lb-°F | |
Special Metals INCONEL® 686 Nickel Superalloy (UNS N06686) Sheet 0.125 in (3.2 mm) Tensile strength (ultimate and yield) and elongation values reported here are typical for 0.125 inch sheet. Other property values are typical of INCONEL® alloy 686.Data provided by the manufacture.. |