Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Special Metals INCONEL® 686 Nickel Superalloy (UNS N06686) Round 1.500 in (38.1 mm)

Category Metal , Nonferrous Metal , Nickel Alloy , Superalloy
Manufacturer Special Metals (includes the former Inco Alloys International Inc.)
Trade Name INCONEL®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Special Metals INCONEL® 686 Nickel Superalloy (UNS N06686) Round 1.500 in (38.1 mm).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Tensile strength (ultimate and yield) and elongation values reported here are typical for 1.500 inch round. Other property values are typical of INCONEL® alloy 686.Data provided by the manufacturer, Special Metals.
Physical Properties Metric English Comments
Density 8.72 g/cc
0.315 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 810.1 MPa
117500 psi
Tensile Strength, Yield 359 MPa

@Strain 0.200 %
52100 psi

@Strain 0.200 %
Elongation at Break 56 %
56 %
Modulus of Elasticity 207 GPa
30000 ksi
Poissons Ratio 0.34
0.34
Shear Modulus 77.0 GPa
11200 ksi
Thermal Properties Metric English Comments
CTE, linear 11.97 µm/m-°C

@Temperature 21.0 - 100 °C
6.650 µin/in-°F

@Temperature 69.8 - 212 °F
Mean
12.56 µm/m-°C

@Temperature 21.0 - 300 °C
6.978 µin/in-°F

@Temperature 69.8 - 572 °F
Mean
13.01 µm/m-°C

@Temperature 21.0 - 500 °C
7.228 µin/in-°F

@Temperature 69.8 - 932 °F
Mean
Specific Heat Capacity 0.373 J/g-°C
0.0891 BTU/lb-°F
Melting Point 1338 - 1380 °C
2440 - 2520 °F
Solidus 1338 °C
2440 °F
Liquidus 1380 °C
2520 °F
Component Elements Properties Metric English Comments
Carbon, C <= 0.010 %
<= 0.010 %
Chromium, Cr 19 - 23 %
19 - 23 %
Iron, Fe <= 5.0 %
<= 5.0 %
Manganese, Mn <= 0.75 %
<= 0.75 %
Molybdenum, Mo 15 - 17 %
15 - 17 %
Nickel, Ni 59 %
59 %
As remainder
Phosphorous, P <= 0.040 %
<= 0.040 %
Sulfur, S <= 0.020 %
<= 0.020 %
Titanium, Ti 0.020 - 0.25 %
0.020 - 0.25 %
Tungsten, W 3.0 - 4.4 %
3.0 - 4.4 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0001237 ohm-cm
0.0001237 ohm-cm
Magnetic Permeability 1.001
1.001
at 200 Oersted (15.9 kA/m)