Specific Heat Capacity 0.381 J/g-°C
0.0910 BTU/lb-°F
Materion moldMAX® XL Spinodally Hardened Copper-Nickel-Tin Alloy
moldMAX XL® is a unique spinodally hardened copper-nickel-tin alloy that combines high strength and high thermal conductivity. Available in large plate thickness up to 12” and in rounds up t..