Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.381 J/g-°C | 0.0910 BTU/lb-°F | |
Materion moldMAX® XL Spinodally Hardened Copper-Nickel-Tin Alloy moldMAX XL® is a unique spinodally hardened copper-nickel-tin alloy that combines high strength and high thermal conductivity. Available in large plate thickness up to 12†and in rounds up t.. |
|||
Specific Heat Capacity | 0.381 J/g-°C | 0.0911 BTU/lb-°F | |
Special Metals INCONEL® alloy 22 Austenitic Alloy INCONEL® alloy 22 (UNS N06022; W.Nr. 2.4602; NiCr21Mo14W) is a fully austenitic advanced corrosion-resistant alloy that offers resistance to both aqueous corrosion and attack at elevated temperat.. |