Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.530 J/g-°C @Temperature 100 °C |
0.127 BTU/lb-°F @Temperature 212 °F |
|
Outokumpu 2205 Duplex Stainless Steel Duplex stainless combining high mechanical strength with good corrosion resistance.Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical t.. |
|||
Specific Heat Capacity | 0.530 J/g-°C @Temperature 500 °C |
0.127 BTU/lb-°F @Temperature 932 °F |
|
Outokumpu 4828 High Temperature Austenitic Stainless Steel Standardized high temperature steel for service at temperatures of up to 950-1000°C in dry air. Utilization in the temperature range of 600-900°C can lead to embrittlement.Applications: Heat and .. |
|||
Specific Heat Capacity | 0.530 J/g-°C @Temperature 500 °C |
0.127 BTU/lb-°F @Temperature 932 °F |
|
Outokumpu 4833 High Temperature Austenitic Stainless Steel Standardized high temperature steel for service at temperatures of up to 950-1000°C in dry air. Utilization in the temperature range of 600-900°C can lead to embrittlement.Applications: Heat and .. |
|||
Specific Heat Capacity | 0.530 J/g-°C @Temperature 500 °C |
0.127 BTU/lb-°F @Temperature 932 °F |
|
Outokumpu 4841 High Temperature Austenitic Stainless Steel Variant of 1.4845 with an increased silicon content which enhances the steel's resistance to oxidation/corrosion but has also made it more susceptible to embrittlement.Applications: Heat and creep r.. |
|||
Specific Heat Capacity | 0.530 J/g-°C @Temperature 500 °C |
0.127 BTU/lb-°F @Temperature 932 °F |
|
Outokumpu 4845 High Temperature Austenitic Stainless Steel Standardized high-temperature steel for use at temperatures up to 1100°C in dry air. Prone to embrittlement after exposure between 600-900°C. Applications: Heat and creep resistance. For use o.. |
|||
Specific Heat Capacity | 0.530 J/g-°C @Temperature 500 °C |
0.127 BTU/lb-°F @Temperature 932 °F |
|
Outokumpu 4878 High Temperature Austenitic Stainless Steel Heat-resistant variant of 1.4541, with a slightly higher max carbon content. Recommended max service temperature for this steel in dry air is 800°C. Applications: Heat and creep resistance. For .. |
|||
Specific Heat Capacity | 0.530 J/g-°C @Temperature 100 °C |
0.127 BTU/lb-°F @Temperature 212 °F |
|
Outokumpu SAF 2304® Duplex Stainless Steel Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical tankersSeawater systemsFirewalls and blast walls on offshore platformsBridgesCompone.. |
|||
Specific Heat Capacity | 0.530 J/g-°C @Temperature 100 °C |
0.127 BTU/lb-°F @Temperature 212 °F |
|
Outokumpu SAF 2507® Duplex Stainless Steel Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical tankersSeawater systemsFirewalls and blast walls on offshore platformsBridgesCompone.. |
|||
Specific Heat Capacity | 0.531 J/g-°C @Temperature 400 °C |
0.127 BTU/lb-°F @Temperature 752 °F |
|
Haynes HR-120® alloy, solution heat-treated Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts .. |
|||
Specific Heat Capacity | 0.531 J/g-°C @Temperature 400 °C |
0.127 BTU/lb-°F @Temperature 752 °F |
|
Haynes HR-120® alloy, solution heat-treated aged at 1200°F for 1000 hours Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts .. |
|||
Specific Heat Capacity | 0.531 J/g-°C @Temperature 400 °C |
0.127 BTU/lb-°F @Temperature 752 °F |
|
Haynes HR-120® alloy, solution heat-treated aged at 1400°F for 1000 hours Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts .. |
|||
Specific Heat Capacity | 0.531 J/g-°C @Temperature 400 °C |
0.127 BTU/lb-°F @Temperature 752 °F |
|
Haynes HR-120® alloy, solution heat-treated aged at 1600°F for 1000 hours Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts .. |
|||
Specific Heat Capacity | 0.531 J/g-°C @Temperature 400 °C |
0.127 BTU/lb-°F @Temperature 752 °F |
|
Haynes HR-120® alloy, solution heat-treated aged at 1800°F for 1000 hours Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts .. |
|||
Specific Heat Capacity | 0.531 J/g-°C @Temperature 400 °C |
0.127 BTU/lb-°F @Temperature 752 °F |
|
Haynes HR-120® alloy, solution heat-treated plate Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts .. |
|||
Specific Heat Capacity | 0.530 J/g-°C | 0.127 BTU/lb-°F | |
Schott N-LASF44 Glass Information Provided by SCHOTT North America, Inc. |
|||
Specific Heat Capacity | 0.530 J/g-°C | 0.127 BTU/lb-°F | |
Schott N-LASF9 Glass Information Provided by SCHOTT North America, Inc. |
|||
Specific Heat Capacity | 0.530 J/g-°C | 0.127 BTU/lb-°F | |
Schott P-SF67 Glass Suitable for precision moldingInformation Provided by SCHOTT North America, Inc. |
|||
Specific Heat Capacity | 0.533 J/g-°C | 0.127 BTU/lb-°F | |
TIMET TIMETAL® 5111 Titanium Alloy (Ti-5Al-1Sn-1Zr-1V-0.8Mo; ASTM Grade 32) High Toughness, Heavy Section Weldable AlloyFeatures: A near alpha alloy with excellent weldability, seawater stress corrosion cracking resistance and high dynamic toughness. It is ideally suited f.. |
|||
Specific Heat Capacity | 0.530 J/g-°C @Temperature 500 °C |
0.127 BTU/lb-°F @Temperature 932 °F |
|
Outokumpu 4948 High Temperature Austenitic Stainless Steel Creep-resistant variant of 1.4301, with a standardized minimum carbon content for service at temperatures of up to 800°C in dry air.Applications: Heat and creep resistance. For use over 550°C for.. |
|||
Specific Heat Capacity | 0.530 J/g-°C @Temperature 100 °C |
0.127 BTU/lb-°F @Temperature 212 °F |
|
Outokumpu LDX 2101® Duplex Stainless Steel Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical tankersSeawater systemsFirewalls and blast walls on offshore platformsBridgesCompone.. |
|||
Specific Heat Capacity | 0.532 J/g-°C @Temperature 400 °C |
0.127 BTU/lb-°F @Temperature 752 °F |
|
Special Metals INCOLOY® Alloy 903 A nickel-iron-cobalt alloy with additions of niobium, titanium, and aluminum for precipitation hardening. The alloy combines high strength with a low and constant coefficient of thermal expansion a.. |