Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.800 J/g-°C | 0.191 BTU/lb-°F | Calculated |
Rogers Corporation RO3010 Ceramic-Filled PTFE Composite, High Frequency Circuit Material Features and Benefits: |
|||
Specific Heat Capacity | 0.800 - 0.840 J/g-°C | 0.191 - 0.201 BTU/lb-°F | |
PEAK Werkstoff DISPAL S270 Aluminum Alloy, AlSi25Fe4Ni3CuMgMnCrTi, Condition F Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational.. |
|||
Specific Heat Capacity | 0.800 J/g-°C @Temperature 20.0 - 100 °C |
0.191 BTU/lb-°F @Temperature 68.0 - 212 °F |
|
Schott Nextrema® 712-6 Glass Ceramic The NEXTREMA® family of glass-ceramics combines the glossy appearance of glass with exceptional thermal, chemical, optical and mechanical properties such as:Very low coefficient of linear thermal.. |
|||
Specific Heat Capacity | 0.800 J/g-°C @Temperature 20.0 - 100 °C |
0.191 BTU/lb-°F @Temperature 68.0 - 212 °F |
|
Schott Nextrema® 724-3 Glass Ceramic The NEXTREMA® family of glass-ceramics combines the glossy appearance of glass with exceptional thermal, chemical, optical and mechanical properties such as:Very low coefficient of linear thermal.. |
|||
Specific Heat Capacity | 0.800 J/g-°C @Temperature 20.0 - 100 °C |
0.191 BTU/lb-°F @Temperature 68.0 - 212 °F |
|
Schott Nextrema® 724-5 Glass Ceramic The NEXTREMA® family of glass-ceramics combines the glossy appearance of glass with exceptional thermal, chemical, optical and mechanical properties such as:Very low coefficient of linear thermal.. |
|||
Specific Heat Capacity | 0.800 J/g-°C @Temperature 20.0 - 100 °C |
0.191 BTU/lb-°F @Temperature 68.0 - 212 °F |
|
Schott Nextrema® 724-8 Glass Ceramic The NEXTREMA® family of glass-ceramics combines the glossy appearance of glass with exceptional thermal, chemical, optical and mechanical properties such as:Very low coefficient of linear thermal.. |
|||
Specific Heat Capacity | 0.800 J/g-°C @Temperature 20.0 - 100 °C |
0.191 BTU/lb-°F @Temperature 68.0 - 212 °F |
|
Schott ROBAX® Glass Ceramic ROBAX® is a highly transparent glass-ceramic having virtually zero thermal expansion and sufficient mechanical resistance required for all standard applications. It is produced in flat, rolled s.. |
|||
Specific Heat Capacity | 0.800 J/g-°C | 0.191 BTU/lb-°F | |
Skamol Group Moler BB-BLOCK Insulating Block SKAMOL Moler insulating bricks & blocks have the following characteristics: Max. service temperature: Up to 1000°C (1832°F)Back-up insulation Excellent insulating propertiesHigh mechanical str.. |
|||
Specific Heat Capacity | 0.800 J/g-°C | 0.191 BTU/lb-°F | |
Skamol Group Moler BF-BLOCK Insulating Block SKAMOL Moler insulating bricks & blocks have the following characteristics: Max. service temperature: Up to 1000°C (1832°F)Back-up insulation Excellent insulating propertiesHigh mechanical str.. |
|||
Specific Heat Capacity | 0.800 J/g-°C | 0.191 BTU/lb-°F | |
Skamol Group Moler M-EXTRA 'E' Insulating Block SKAMOL Moler insulating bricks & blocks have the following characteristics: Max. service temperature: Up to 1000°C (1832°F)Back-up insulation Excellent insulating propertiesHigh mechanical str.. |
|||
Specific Heat Capacity | 0.800 J/g-°C | 0.191 BTU/lb-°F | |
Skamol Group Moler POROS Insulating Block SKAMOL Moler insulating bricks & blocks have the following characteristics: Max. service temperature: Up to 1000°C (1832°F)Back-up insulation Excellent insulating propertiesHigh mechanical str.. |
|||
Specific Heat Capacity | 0.800 J/g-°C | 0.191 BTU/lb-°F | |
Skamol Group Moler ROTOL Insulating Block SKAMOL Moler insulating bricks & blocks have the following characteristics: Max. service temperature: Up to 1000°C (1832°F)Back-up insulation Excellent insulating propertiesHigh mechanical str.. |
|||
Specific Heat Capacity | 0.800 J/g-°C | 0.191 BTU/lb-°F | |
Skamol Group Moler SUPRA Insulating Block SKAMOL Moler insulating bricks & blocks have the following characteristics: Max. service temperature: Up to 1000°C (1832°F)Back-up insulation Excellent insulating propertiesHigh mechanical str.. |
|||
Specific Heat Capacity | 0.800 J/g-°C | 0.191 BTU/lb-°F | |
Sapco 99.7% Aluminum Oxide Information provided by Sapco. |
|||
Specific Heat Capacity | 0.800 J/g-°C | 0.191 BTU/lb-°F | |
Sapco 99.9% Aluminum Oxide Information provided by Sapco. |
|||
Specific Heat Capacity | 0.800 J/g-°C | 0.191 BTU/lb-°F | |
Schott N-LAF34 Glass Information Provided by SCHOTT North America, Inc. |
|||
Specific Heat Capacity | 0.800 J/g-°C | 0.191 BTU/lb-°F | |
Skamol Group Moler SM-65 Insulating Block SKAMOL Moler insulating bricks & blocks have the following characteristics: Max. service temperature: Up to 1000°C (1832°F)Back-up insulation Excellent insulating propertiesHigh mechanical str.. |
|||
Specific Heat Capacity | 0.800 J/g-°C @Temperature 32.0 - 800 °C |
0.191 BTU/lb-°F @Temperature 89.6 - 1470 °F |
|
Unifrax Excelfrax® 1800 Board Microporous Insulation Unifrax Corporation's Excelfrax® product line, based on advanced microporous insulation technology, is a family of products which all exhibit superior insulating characteristics. Excelfrax micropo.. |
|||
Specific Heat Capacity | 0.800 J/g-°C @Temperature 32.0 - 800 °C |
0.191 BTU/lb-°F @Temperature 89.6 - 1470 °F |
|
Unifrax Excelfrax® 1800 Flexliner Microporous Insulation Unifrax Corporation's Excelfrax® product line, based on advanced microporous insulation technology, is a family of products which all exhibit superior insulating characteristics. Excelfrax micropo.. |
|||
Specific Heat Capacity | 0.800 J/g-°C @Temperature 32.0 - 800 °C |
0.191 BTU/lb-°F @Temperature 89.6 - 1470 °F |
|
Unifrax Excelfrax® 200 VIP Vacuum Insulation Panel Excelfrax® 200 VIP is a Vaccum Insulation Panel (VIP) designed to provide insulation at temperatures between -300°F and +300°F. This thermal insulation provides extremely low thermal conductivit.. |
|||
Specific Heat Capacity | 0.800 J/g-°C | 0.191 BTU/lb-°F | DINV ENV 821-3 |
CeramTec DN 70 Dispersion Ceramic, Al2O3-ZrO2 DN 70 is a ZTA Alumina Toughened Zirconia. |
|||
Specific Heat Capacity | 0.800 J/g-°C @Temperature 100 - 200 °C |
0.191 BTU/lb-°F @Temperature 212 - 392 °F |
DINV ENV 821-3 |
CeramTec Rubalit® 708S Alumina, 96% Rubalit® 708S (96%) is an alumina that features high strength and thermal conductivity. It provides outstanding results when used on commercially available thick-film pastes and metallization syste.. |
|||
Specific Heat Capacity | 0.800 J/g-°C @Temperature 20.0 - 100 °C |
0.191 BTU/lb-°F @Temperature 68.0 - 212 °F |
|
CeramTec Ziralit Zirconia Toughened Alumina (ZTA), Al2O3•ZrO2 CeramTec's Zirconia Toughened Alumina (Ziralit) provides excellent strength, excellent temperature performance, and superior toughness. It has enhanced performance for high quantity volume productio.. |
|||
Specific Heat Capacity | 0.800 J/g-°C | 0.191 BTU/lb-°F | |
CeramTec CeramCool® Rubalit® 708 Alumina, 96% CeramCool® is a metallized ceramic heat-sink for high power applications demonstrated by high power LED-systems. CeramCool® material characteristics: electrical insulation, high volume resistivit.. |