CeramTec's Zirconia Toughened Alumina (Ziralit) provides excellent strength, excellent temperature performance, and superior toughness. It has enhanced performance for high quantity volume production and tight tolerances designs. Ziralit provides considerable improvement in strength and toughness over standard silicate products used in the fuse market. Due to its high temperature performance, the material has demonstrated successful application in the telecommunication fuse market where demanding requirements of 600V and 60A are typical.
Physical Properties Metric English Comments
Density 3.80 g/cc
0.137 lb/in³
Water Absorption 0.00 %
0.00 %
Mechanical Properties Metric English Comments
Modulus of Elasticity 200 GPa
29000 ksi
Flexural Strength 335 MPa
48600 psi
4 point
Thermal Properties Metric English Comments
CTE, linear 7.60 µm/m-°C

@Temperature 20.0 - 200 °C
4.22 µin/in-°F

@Temperature 68.0 - 392 °F
8.20 µm/m-°C

@Temperature 20.0 - 500 °C
4.56 µin/in-°F

@Temperature 68.0 - 932 °F
Specific Heat Capacity 0.800 J/g-°C

@Temperature 20.0 - 100 °C
0.191 BTU/lb-°F

@Temperature 68.0 - 212 °F
Thermal Conductivity 13.0 W/m-K

@Temperature 20.0 - 100 °C
90.2 BTU-in/hr-ft²-°F

@Temperature 68.0 - 212 °F
Electrical Properties Metric English Comments
Volume Resistivity 5.30e+7 ohm-cm

@Temperature 600 °C
5.30e+7 ohm-cm

@Temperature 1110 °F
1.40e+13 ohm-cm

@Temperature 100 °C
1.40e+13 ohm-cm

@Temperature 212 °F
8.80e+15 ohm-cm

@Temperature 20.0 °C
8.80e+15 ohm-cm

@Temperature 68.0 °F
Dielectric Strength 30.0 kV/mm
762 kV/in
Descriptive Properties Value Comments
Color White
Thermal Shock Resistance R1 (K) 130
Withstand Voltage (kV) > 15