Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.200 J/g-°C | 0.0478 BTU/lb-°F | |
Mateck Cesium Iodide, CsI Optical crystals |
|||
Specific Heat Capacity | 0.200 - 0.480 J/g-°C | 0.0478 - 0.115 BTU/lb-°F | |
Goodfellow Tungsten Carbide/Cobalt Tungsten Carbide is a hard, brittle ceramic which, when combined with 6% to 10% Cobalt, forms a tough Cermet (Ceramic-Metal). This material was developed for use in cutting tools, having hard cerami.. |
|||
Specific Heat Capacity | <= 0.200 J/g-°C | <= 0.0478 BTU/lb-°F | |
Alliance BIF-11 Bonded (Composite) Magnetic Material |
|||
Specific Heat Capacity | <= 0.200 J/g-°C | <= 0.0478 BTU/lb-°F | |
Alliance BIF-17 Bonded (Composite) Magnetic Material |
|||
Specific Heat Capacity | <= 0.200 J/g-°C | <= 0.0478 BTU/lb-°F | |
Alliance BIF-19 Bonded (Composite) Magnetic Material |
|||
Specific Heat Capacity | <= 0.200 J/g-°C | <= 0.0478 BTU/lb-°F | |
Alliance BIF-2 Bonded (Composite) Magnetic Material |
|||
Specific Heat Capacity | <= 0.200 J/g-°C | <= 0.0478 BTU/lb-°F | |
Alliance BIF-16 Bonded (Composite) Magnetic Material |
|||
Specific Heat Capacity | 0.200 J/g-°C @Temperature 20.0 °C |
0.0478 BTU/lb-°F @Temperature 68.0 °F |
|
Industeel URANUS® S1 4 % Si, Austenitic Stainless Steel Resistant to Nitric Acid Solutions Description: Research carried out in about the last fifteen years in CREUSOT LOIRE INDUSTRIE laboratories shows that a strong addition of silicon to austenitic stainless steels of the 18/10 type has.. |