Industeel URANUS® S1 4 % Si, Austenitic Stainless Steel Resistant to Nitric Acid Solutions

Category Metal , Ferrous Metal , Austenitic , Stainless Steel , T S30000 Series Stainless Steel
Manufacturer Groupe Arcelor
Trade Name URANUS®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Industeel URANUS® S1 4 % Si, Austenitic Stainless Steel Resistant to Nitric Acid Solutions.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Research carried out in about the last fifteen years in CREUSOT LOIRE INDUSTRIE laboratories shows that a strong addition of silicon to austenitic stainless steels of the 18/10 type has a favorable influence on resistance to transpassive intergranular corrosion. This type of corrosion develops particularly in very concentrated nitric environments (> 90 %) up to boiling point, also in strongly oxidizing nitric environments (oxidizing ions present such as : hexavalentchromic pentavalent vanadium - ferritic salts etc...). URANUS® S1 steel grade puts in a concrete form the results of research in this domain.Information provided by manufacturer.
Physical Properties Metric English Comments
Density 7.70 g/cc
0.278 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate >= 530 MPa
>= 76900 psi
Minimum Guaranteed
Tensile Strength, Yield >= 260 MPa

@Strain 1.00 %
>= 37700 psi

@Strain 1.00 %
>= 280 MPa

@Strain 0.200 %
>= 40600 psi

@Strain 0.200 %
Elongation at Break >= 45 %
>= 45 %
Modulus of Elasticity 200 GPa
29000 ksi
Poissons Ratio 0.22
0.22
Calculated
Shear Modulus 82.0 GPa

@Temperature 20.0 °C
11900 ksi

@Temperature 68.0 °F
Thermal Properties Metric English Comments
CTE, linear 16.5 µm/m-°C

@Temperature 20.0 - 100 °C
9.17 µin/in-°F

@Temperature 68.0 - 212 °F
18.0 µm/m-°C

@Temperature 20.0 - 300 °C
10.0 µin/in-°F

@Temperature 68.0 - 572 °F
19.0 µm/m-°C

@Temperature 20.0 - 500 °C
10.6 µin/in-°F

@Temperature 68.0 - 932 °F
Specific Heat Capacity 0.200 J/g-°C

@Temperature 20.0 °C
0.0478 BTU/lb-°F

@Temperature 68.0 °F
Component Elements Properties Metric English Comments
Carbon, C <= 0.015 %
<= 0.015 %
Chromium, Cr 17 %
17 %
Iron, Fe 64.485 - 64.5 %
64.485 - 64.5 %
As remainder
Nickel, Ni 14.5 %
14.5 %
Silicon, Si 4.0 %
4.0 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000750 ohm-cm

@Temperature 20.0 °C
0.0000750 ohm-cm

@Temperature 68.0 °F