Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.946 - 0.962 J/g-°C | 0.226 - 0.230 BTU/lb-°F | Average value: 0.960 J/g-°C Grade Count:15 |
Overview of materials for ECTFE Fluoropolymer This property data is a summary of similar materials in the MatWeb database for the category "ECTFE Fluoropolymer". Each property range of values reported is minimum and maximum values of appropriat.. |