Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 1.103 J/g-°C | 0.2636 BTU/lb-°F | Liquid |
3M Novec™ 612 Magnesium Protection Fluid Novec 612 fluid, dodecafluoro-2-methyl-3-pentanone or (CF3CF2C(O)CF(CF3)2, is a clear, colorless, and low odor fluid. Its properties, environmental profile, and margin of safety make it a sustainabl.. |
|||
Specific Heat Capacity | 1.103 J/g-°C | 0.2636 BTU/lb-°F | Liquid |
3M Novec™ 1230 Fire Protection Fluid 3M™ Novec™ 1230 Fire Protection Fluid is a next-generation halon and HFC clean agent replacement technology, designed to alleviate concerns for human safety, performance and the environment.Featur.. |
|||
Specific Heat Capacity | 1.103 J/g-°C | 0.2636 BTU/lb-°F | |
3M Novec™ 649 Engineered Fluid 3M™ Novec™ 649 Engineered Fluid is a clear, colorless and low odor fluid, one in a line of 3M products designed as replacements for ozone depleting substances (ODSs) and compounds with high global.. |