Material Notes:
3M™ Novec™ 1230 Fire Protection Fluid is a next-generation halon and HFC clean agent replacement technology, designed to alleviate concerns for human safety, performance and the environment.Features and Benefits:Next generation halon and HFC clean agent replacement technologyZero ozone depletion potential5-day atmospheric lifetimeGlobal warming potential of 1Largest margin of safety among chemical clean agents for occupied spacesInformation provided by 3M
Physical Properties Metric English Comments
Density 1.60 g/cc
0.0578 lb/in³
Sat. Liquid
0.891 g/cc

@Pressure 0.101 MPa
0.0322 lb/in³

@Pressure 14.7 psi
gas
Viscosity Measure 0.39 cSt

@Temperature 25.0 °C
0.39 cSt

@Temperature 77.0 °F
Liquid
0.56 cSt

@Temperature 0.000 °C
0.56 cSt

@Temperature 32.0 °F
Liquid
Molecular Weight 316.04 g/mol
316.04 g/mol
Vapor Pressure 0.404 bar
303 torr
Thermal Properties Metric English Comments
Heat of Vaporization 88.0 J/g
37.9 BTU/lb
@ boiling point
Specific Heat Capacity 1.103 J/g-°C
0.2636 BTU/lb-°F
Liquid
0.0987 J/g-°C

@Pressure 0.101 MPa
0.0236 BTU/lb-°F

@Pressure 14.7 psi
Vapor
Boiling Point 49.2 °C

@Pressure 0.101 MPa
121 °F

@Pressure 14.7 psi
Chemical Properties Metric English Comments
Critical Pressure 18.65 bar
13990 torr
Critical Temperature 168.7 °C
335.7 °F
Critical Density 0.639 g/cc
0.0231 lb/in³
Critical Molar Volume 494.5 cm³/mol
30.18 in³/mol
Descriptive Properties Value Comments
Relative Dielectric Strength 2.3
1 atm (N<sub>2</sub>=1.0)