Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.335 J/g-°C | 0.0800 BTU/lb-°F | ASTM D1269E |
Premix Premi-Glas® 8201-24 Glass Reinforced Polyester SMC
(discontinued **) Description: Premi-Glas® 8201-24 is a low profile glass reinforced polyester Sheet Molding Compound designed for body panel applications.Key features and benefits: Compatible with in-mold coatings,.. |
|||
Specific Heat Capacity | 0.335 J/g-°C | 0.0801 BTU/lb-°F | |
Special Metals UDIMAR® alloy 300 Fe-Ni Maraging Steel UDIMAR® alloy 300 (UNS K93120) is an age-hardenable (maraging) iron-nickel steel combining ultra-high strength, toughness and resistance to crack propagation. The alloy is well suited to applica.. |
|||
Specific Heat Capacity | 0.335 J/g-°C | 0.0800 BTU/lb-°F | |
Premix Premi-Glas® 7203-28 28% Glass Reinforced Polyester SMC
(discontinued **) Description: Premi-Glas® 7203-28 is a low profile, 28% glass reinforced polyester Sheet Molding Compound designed for automotive structural vehicle body panel applications that require high flexura.. |