Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 1.13 - 1.55 J/g-°C | 0.270 - 0.370 BTU/lb-°F | Average value: 1.43 J/g-°C Grade Count:4 |
Overview of materials for Polycarbonate, 20% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 20% Glass Filled". Specific grades with glass content between 15% and 24% are included. E.. |