Thermal Properties Metric English Comments
Specific Heat Capacity 1.26 - 1.70 J/g-°C

@Temperature 50.0 - 200 °C
0.301 - 0.406 BTU/lb-°F

@Temperature 122 - 392 °F
Average value: 1.47 J/g-°C Grade Count:5
Overview of materials for Polyaryletherketone (PAEK), Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyaryletherketone (PAEK), Glass Fiber Filled". Each property range of values reported is minimum and m..
Specific Heat Capacity 1.17 - 1.70 J/g-°C
0.280 - 0.406 BTU/lb-°F
Average value: 1.36 J/g-°C Grade Count:3
Overview of materials for Polycarbonate, Optical Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Optical Grade". Each property range of values reported is minimum and maximum values of a..