Specific Heat Capacity 0.456 J/g-°C
0.109 BTU/lb-°F
Mateck Barium Fluoride, BaF2
Optical crystals
Specific Heat Capacity 0.456 J/g-°C
0.109 BTU/lb-°F
Special Metals Nickel 200
Commercially pure (99.6%) wrought nickel with good mechanical properties and resistance to a range of corrosive media. Good thermal, electrical, and magnetostrictive properties. Ferromagnetic. Us..
Specific Heat Capacity 0.456 J/g-°C
0.109 BTU/lb-°F
Special Metals Nickel 201
Commercially pure (99.6%) wrought nickel essentially the same as Nickel 200 but with a lower carbon content to prevent embrittlement by intergranular carbon at temperatures over 600°F (315°C)...
Specific Heat Capacity 0.456 J/g-°C
0.109 BTU/lb-°F
Special Metals Nickel 205
Wrought nickel similar to Nickel 200 but with compositional adjustments to enhance performance in electrical and electronic applications. Ferromagnetic. Used for the anodes and grids of electronic..
Specific Heat Capacity 0.456 J/g-°C

@Temperature 20.0 °C
0.109 BTU/lb-°F

@Temperature 68.0 °F
California Fine Wire Nickel A 200 Nickel Alloy
All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire.
Specific Heat Capacity 0.456 J/g-°C
0.109 BTU/lb-°F
ATI Allegheny Ludlum AL 200™ Nickel Alloy, UNS N02200
Ferromagnetic. Allegheny Ludlum AL 200 alloy is wrought commercially pure nickel. This alloy provides highly ductile mechanical properties across a wide temperature range. Either alloy provides c..
Specific Heat Capacity 0.456 J/g-°C
0.109 BTU/lb-°F
ATI Allegheny Ludlum AL 201™ Nickel Alloy, UNS N02201
Ferromagnetic. Allegheny Ludlum AL 201 alloy is wrought commercially pure nickel. This alloy provides highly ductile mechanical properties across a wide temperature range. Either alloy provides c..