Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.467 J/g-°C | 0.112 BTU/lb-°F | RT |
Haynes HR-120® alloy, solution heat-treated Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts .. |
|||
Specific Heat Capacity | 0.467 J/g-°C | 0.112 BTU/lb-°F | RT |
Haynes HR-120® alloy, solution heat-treated aged at 1200°F for 1000 hours Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts .. |
|||
Specific Heat Capacity | 0.467 J/g-°C | 0.112 BTU/lb-°F | RT |
Haynes HR-120® alloy, solution heat-treated aged at 1400°F for 1000 hours Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts .. |
|||
Specific Heat Capacity | 0.467 J/g-°C | 0.112 BTU/lb-°F | RT |
Haynes HR-120® alloy, solution heat-treated aged at 1600°F for 1000 hours Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts .. |
|||
Specific Heat Capacity | 0.467 J/g-°C | 0.112 BTU/lb-°F | RT |
Haynes HR-120® alloy, solution heat-treated aged at 1800°F for 1000 hours Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts .. |
|||
Specific Heat Capacity | 0.467 J/g-°C | 0.112 BTU/lb-°F | RT |
Haynes HR-120® alloy, solution heat-treated plate Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts .. |