Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 1.96 J/g-°C | 0.468 BTU/lb-°F | |
Styron CALIBRE™ 300 15 Polycarbonate, General Purpose CALIBRE® 300 series are general purpose, UL listed polycarbonate resins. CALIBRE 300 series resins exhibit an excellent physical property balance of heat resistance, transparency and impact stren.. |
|||
Specific Heat Capacity | 1.96 J/g-°C | 0.468 BTU/lb-°F | |
Styron CALIBRE™ 300 4 Polycarbonate, General Purpose CALIBRE® 300 series are general purpose, UL listed polycarbonate resins. CALIBRE 300 series resins exhibit an excellent physical property balance of heat resistance, transparency and impact stren.. |
|||
Specific Heat Capacity | 1.96 J/g-°C | 0.468 BTU/lb-°F | |
Styron CALIBRE™ 300 6 Polycarbonate, General Purpose CALIBRE® 300 series are general purpose, UL listed polycarbonate resins. CALIBRE 300 series resins exhibit an excellent physical property balance of heat resistance, transparency and impact stren.. |
|||
Specific Heat Capacity | 1.96 J/g-°C | 0.468 BTU/lb-°F | |
Styron CALIBRE™ 300EP 22 Polycarbonate, General Purpose CALIBRE® 300EP series resins are general purpose polycarbonate resins and can be supplied with a mold release package, a UV stabilizer package or both. CALIBRE 300EP resins exhibit an excellent p.. |
|||
Specific Heat Capacity | 1.96 J/g-°C | 0.468 BTU/lb-°F | |
Styron Magnum™ 9030 ABS, High Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Specific Heat Capacity | 1.96 J/g-°C @Temperature 180 °C |
0.468 BTU/lb-°F @Temperature 356 °F |
Liquid (Unpolymerized resin); ASTM E1269 |
Cyclics CBT® 100 Thermoplastic Resin CBT® 100 resin melts to a water-like viscosity when heated, then polymerizes into the engineering thermoplastic resin polybutylene terephthalate (PBT). CBT 200 resin has a processing range between.. |
|||
Specific Heat Capacity | 1.96 J/g-°C @Temperature 180 °C |
0.468 BTU/lb-°F @Temperature 356 °F |
Liquid (Unpolymerized resin); ASTM E1269 |
Cyclics CBT® 200 Thermoplastic Resin CBT® 200 resin melts to a water-like viscosity when heated, then polymerizes into the engineering thermoplastic resin polybutylene terephthalate (PBT). CBT 200 resin has a processing range between.. |
|||
Specific Heat Capacity | 1.96 J/g-°C | 0.468 BTU/lb-°F | Melt value |
BASF Capron® 8333G HI Impact Modified, 33% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron 8333G HI is a 33% glass reinforced, impact modified polyamide 6 injection molding compound developed for applications requiring improved dry as molded toughness in combination with a balance .. |