Specific Heat Capacity 0.663 J/g-°C

@Temperature 1000 °C
0.158 BTU/lb-°F

@Temperature 1830 °F
Haynes HR-120® alloy, solution heat-treated
Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts ..
Specific Heat Capacity 0.663 J/g-°C

@Temperature 1000 °C
0.158 BTU/lb-°F

@Temperature 1830 °F
Haynes HR-120® alloy, solution heat-treated aged at 1200°F for 1000 hours
Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts ..
Specific Heat Capacity 0.663 J/g-°C

@Temperature 1000 °C
0.158 BTU/lb-°F

@Temperature 1830 °F
Haynes HR-120® alloy, solution heat-treated aged at 1400°F for 1000 hours
Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts ..
Specific Heat Capacity 0.663 J/g-°C

@Temperature 1000 °C
0.158 BTU/lb-°F

@Temperature 1830 °F
Haynes HR-120® alloy, solution heat-treated aged at 1600°F for 1000 hours
Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts ..
Specific Heat Capacity 0.663 J/g-°C

@Temperature 1000 °C
0.158 BTU/lb-°F

@Temperature 1830 °F
Haynes HR-120® alloy, solution heat-treated aged at 1800°F for 1000 hours
Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts ..
Specific Heat Capacity 0.663 J/g-°C

@Temperature 1000 °C
0.158 BTU/lb-°F

@Temperature 1830 °F
Haynes HR-120® alloy, solution heat-treated plate
Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts ..