Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.794 J/g-°C | 0.190 BTU/lb-°F | |
Osprey Metals CE11 Al-Si Controlled Expansion Alloy Al-50%Si controlled expansion alloy manufactured and patented by Osprey Metals Ltd.Information provided to MatWeb by Osprey Metals. |
|||
Specific Heat Capacity | 0.794 J/g-°C | 0.190 BTU/lb-°F | |
Momentive Performance Materials PolarTherm® PT110 Boron Nitride (BN) Powder Fine Hexagonal BN PowderWhen used in a variety of polymeric materials, PolarTherm™'s heat dissipating capability helps extend the service life and enhance the reliability of electronic comp.. |
|||
Specific Heat Capacity | 0.794 J/g-°C | 0.190 BTU/lb-°F | |
Momentive Performance Materials PolarTherm® PT120 Boron Nitride (BN) Powder Fine Hexagonal BN PowderWhen used in a variety of polymeric materials, PolarTherm™'s heat dissipating capability helps extend the service life and enhance the reliability of electronic comp.. |
|||
Specific Heat Capacity | 0.794 J/g-°C | 0.190 BTU/lb-°F | |
Momentive Performance Materials PolarTherm® PT140 Boron Nitride (BN) Powder Fine Hexagonal BN PowderWhen used in a variety of polymeric materials, PolarTherm™'s heat dissipating capability helps extend the service life and enhance the reliability of electronic componen.. |
|||
Specific Heat Capacity | 0.794 J/g-°C | 0.190 BTU/lb-°F | |
Momentive Performance Materials PolarTherm® PT160 Boron Nitride (BN) Powder Fine Hexagonal BN PowderWhen used in a variety of polymeric materials, PolarTherm™'s heat dissipating capability helps extend the service life and enhance the reliability of electronic componen.. |
|||
Specific Heat Capacity | 0.794 J/g-°C | 0.190 BTU/lb-°F | |
Momentive Performance Materials PolarTherm® PT180 Boron Nitride (BN) Powder Fine Hexagonal BN PowderWhen used in a variety of polymeric materials, PolarTherm™'s heat dissipating capability helps extend the service life and enhance the reliability of electronic componen.. |
|||
Specific Heat Capacity | 0.794 J/g-°C | 0.190 BTU/lb-°F | |
Momentive Performance Materials PolarTherm® PT350 Boron Nitride (BN) Powder Low Density BN AgglomerateWhen used in a variety of polymeric materials, PolarTherm™'s heat dissipating capability helps extend the service life and enhance the reliability of electronic compon.. |
|||
Specific Heat Capacity | 0.794 J/g-°C | 0.190 BTU/lb-°F | |
Momentive Performance Materials PolarTherm® PT370 Boron Nitride (BN) Powder Low Density BN AgglomerateWhen used in a variety of polymeric materials, PolarTherm™'s heat dissipating capability helps extend the service life and enhance the reliability of electronic compon.. |
|||
Specific Heat Capacity | 0.794 J/g-°C | 0.190 BTU/lb-°F | |
Momentive Performance Materials PolarTherm® PT620 Boron Nitride (BN) Powder High Density BN AgglomerateWhen used in a variety of polymeric materials, PolarTherm™'s heat dissipating capability helps extend the service life and enhance the reliability of electronic comp.. |
|||
Specific Heat Capacity | 0.794 J/g-°C | 0.190 BTU/lb-°F | |
Momentive Performance Materials PolarTherm® PT670 Boron Nitride (BN) Powder High Density BN AgglomerateWhen used in a variety of polymeric materials, PolarTherm™'s heat dissipating capability helps extend the service life and enhance the reliability of electronic comp.. |