Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.950 J/g-°C | 0.227 BTU/lb-°F | Calculated |
Rogers Corporation RO3203 Woven-Glass Reinforced PTFE Laminate Features and Benefits:Woven glass reinforcement - Improves rigidity for easier handlingUniform electrical and mechanical performance - ideal for complex multi-layer high frequency structuresLow diel.. |
|||
Specific Heat Capacity | 0.950 J/g-°C | 0.227 BTU/lb-°F | calculated |
Rogers Corporation RT/duroid® 5880LZ Lightweight, High Frequency PTFE Laminate RT/duroid® 5880LZ filled PTFE composites are designed for exacting stripline and microstrip circuit applications. The unique filler results in a low density, lightweight material for high performa.. |
|||
Specific Heat Capacity | 0.950 J/g-°C | 0.227 BTU/lb-°F | vapor |
Solvay Chemicals Allyl chloride 3-chloropropene Allyl chloride is mainly used in the manufacture of epichlorohydrin. It is also used in the production of allylic ethers, esters, silanes and quaternary ammonium derivatives.EINECS Number: 203-457-6.. |
|||
Specific Heat Capacity | 0.950 J/g-°C | 0.227 BTU/lb-°F | vapor |
Solvay Chemicals Allyl chloride High purity – Non stabilized 3-chloropropene Allyl chloride is mainly used in the manufacture of epichlorohydrin. It is also used in the production of allylic ethers, esters, silanes and quaternary ammonium derivatives.EINECS Number: 203-457-6.. |
|||
Specific Heat Capacity | 0.950 J/g-°C | 0.227 BTU/lb-°F | vapor |
Solvay Chemicals Allyl chloride High purity 3-chloropropene Allyl chloride is mainly used in the manufacture of epichlorohydrin. It is also used in the production of allylic ethers, esters, silanes and quaternary ammonium derivatives.EINECS Number: 203-457-6.. |
|||
Specific Heat Capacity | 0.950 J/g-°C | 0.227 BTU/lb-°F | ASTM E1269 |
CoorsTek Mullite, S2 Thermal Shock Delta Tc = 300°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Specific Heat Capacity | 0.950 J/g-°C | 0.227 BTU/lb-°F | |
AMT AM-Lite® Die Casting Magnesium Alloy AM-lite is a high surface finish die casting alloy suitable for applications that currently utilize zinc, aluminum or magnesium (alloy AZ91D) die castings, or plastic injection moldings. AM-lite has.. |