Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

CoorsTek Mullite, S2

Category Ceramic , Oxide , Aluminum Oxide
Manufacturer CoorsTek
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CoorsTek Mullite, S2.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Thermal Shock Delta Tc = 300°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a sharp decrease in the flexural strength of the sample.Corrosion: Although all Coors Ceramics are highly resistant to chemical attack, Coors recommends obtaining specific application data from Coors before design finalization.Data Provided by the manufacturer, Coors Ceramics Co.
Physical Properties Metric English Comments
Density 2.80 g/cc
0.101 lb/in³
ASTM C20
Water Absorption 0.00 %
0.00 %
ASTM C373
Particle Size 10 µm
10 µm
Average Crystal Size - Thin Section Test
Mechanical Properties Metric English Comments
Knoop Microhardness 7.4
7.4
1000 g load
Hardness, Rockwell 45 N 70
70
GPa
Modulus of Elasticity 150 GPa
21800 ksi
ASTM C848
Flexural Strength 170 MPa
24700 psi
ASTM F417
Compressive Strength 550 MPa
79800 psi
ASTM C773
Poissons Ratio 0.25
0.25
ASTM C848
Fracture Toughness 2.00 MPa-m½
1.82 ksi-in½
Notched Beam
Shear Modulus 60.0 GPa
8700 ksi
Calculated
Thermal Properties Metric English Comments
CTE, linear 5.30 µm/m-°C

@Temperature 25.0 - 1000 °C
2.94 µin/in-°F

@Temperature 77.0 - 1830 °F
ASTM C372
Specific Heat Capacity 0.950 J/g-°C
0.227 BTU/lb-°F
ASTM E1269
Thermal Conductivity 3.50 W/m-K
24.3 BTU-in/hr-ft²-°F
ASTM C408
Maximum Service Temperature, Air 1700 °C
3090 °F
No Load
Electrical Properties Metric English Comments
Electrical Resistivity >= 1.00e+13 ohm-cm
>= 1.00e+13 ohm-cm
ASTM D1829
300000 ohm-cm

@Temperature 1000 °C
300000 ohm-cm

@Temperature 1830 °F
ASTM D1829
5.00e+12 ohm-cm

@Temperature 500 °C
5.00e+12 ohm-cm

@Temperature 932 °F
ASTM D1829
Dielectric Constant 6.0

@Frequency 1e+6 Hz
6.0

@Frequency 1e+6 Hz
Dielectric Strength 9.80 kV/mm
249 kV/in
ac; ASTM D116
Dielectric Loss Index 0.0020
0.0020
at 25°C, 1 MHz; ASTM D2520
Descriptive Properties Value Comments
Color Tan
Users viewing this material also viewed the following: