Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.973 J/g-°C | 0.233 BTU/lb-°F | |
Solvay Specialty Polymers Galden® D02 PFPE Fluid Galden® D grades are specifically recommended for electronic reliability testing, including thermal shock and hermetic seal testing.Galden® PFPE is a line of high-performance, inert, fluorinat.. |
|||
Specific Heat Capacity | 0.973 J/g-°C | 0.233 BTU/lb-°F | |
Solvay Specialty Polymers Galden® D02TS PFPE Fluid Galden® D grades are specifically recommended for electronic reliability testing, including thermal shock and hermetic seal testing.Galden® PFPE is a line of high-performance, inert, fluorinat.. |
|||
Specific Heat Capacity | 0.973 J/g-°C | 0.233 BTU/lb-°F | |
Solvay Specialty Polymers Galden® D03 PFPE Fluid Galden® D grades are specifically recommended for electronic reliability testing, including thermal shock and hermetic seal testing.Galden® PFPE is a line of high-performance, inert, fluorinat.. |
|||
Specific Heat Capacity | 0.973 J/g-°C | 0.233 BTU/lb-°F | |
Solvay Specialty Polymers Galden® D05 PFPE Fluid Galden® D grades are specifically recommended for electronic reliability testing, including thermal shock and hermetic seal testing.Galden® PFPE is a line of high-performance, inert, fluorinat.. |
|||
Specific Heat Capacity | 0.973 J/g-°C | 0.233 BTU/lb-°F | |
Solvay Specialty Polymers Galden® DET PFPE Fluid Galden® D grades are specifically recommended for electronic reliability testing, including thermal shock and hermetic seal testing.Galden® PFPE is a line of high-performance, inert, fluorinat.. |
|||
Specific Heat Capacity | 0.973 J/g-°C | 0.233 BTU/lb-°F | |
Solvay Specialty Polymers Galden® HS240 PFPE VPS Fluid Galden® LS and HS grades are specifically recommended for vapor phase soldering.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of servic.. |
|||
Specific Heat Capacity | 0.973 J/g-°C | 0.233 BTU/lb-°F | |
Solvay Specialty Polymers Galden® HS260 PFPE VPS Fluid Galden® LS and HS grades are specifically recommended for vapor phase soldering.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of servic.. |
|||
Specific Heat Capacity | 0.973 J/g-°C | 0.233 BTU/lb-°F | |
Solvay Specialty Polymers Galden® LLS215 PFPE VPS Fluid Galden® LS and HS grades are specifically recommended for vapor phase soldering.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of servic.. |
|||
Specific Heat Capacity | 0.973 J/g-°C | 0.233 BTU/lb-°F | |
Solvay Specialty Polymers Galden® LS200 PFPE VPS Fluid Galden® LS and HS grades are specifically recommended for vapor phase soldering.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of servic.. |
|||
Specific Heat Capacity | 0.973 J/g-°C | 0.233 BTU/lb-°F | |
Solvay Specialty Polymers Galden® LS230 PFPE VPS Fluid Galden® LS and HS grades are specifically recommended for vapor phase soldering.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of servic.. |