Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Specialty Polymers Galden® D02 PFPE Fluid

Category Fluid , Polymer
Manufacturer Solvay Specialty Polymers (former Solexis)
Trade Name Galden®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Galden® D02 PFPE Fluid.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Galden® D grades are specifically recommended for electronic reliability testing, including thermal shock and hermetic seal testing.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of service temperature ranges, are available. Uses include heat transfer, electronic reliability testing, vapor phase soldering, solvents, and acid spill mitigation.
Physical Properties Metric English Comments
Density 1.54 g/cc

@Temperature 125 °C
0.0556 lb/in³

@Temperature 257 °F
1.77 g/cc

@Temperature 25.0 °C
0.0639 lb/in³

@Temperature 77.0 °F
1.95 g/cc

@Temperature -54.0 °C
0.0704 lb/in³

@Temperature -65.2 °F
Kinematic Viscosity 1.8 cSt

@Temperature 25.0 °C
1.8 cSt

@Temperature 77.0 °F
Molecular Weight 760 g/mol
760 g/mol
average
Surface Tension 16 dynes/cm
16 dynes/cm
Thermal Properties Metric English Comments
CTE, linear 367 µm/m-°C
204 µin/in-°F
converted from volumetric expansion of 0.0011 cm<sup>3</sup>/cm<sup>3</sup>-°C
Specific Heat Capacity 0.973 J/g-°C
0.233 BTU/lb-°F
Thermal Conductivity 0.0700 W/m-K
0.486 BTU-in/hr-ft²-°F
Boiling Point 175 °C
347 °F
Pour Point -97.0 °C
-143 °F
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
Dielectric Constant 2.1
2.1
Dielectric Strength 15.7 kV/mm
399 kV/in
2.54 mm gap