Thermal Properties Metric English Comments
Specific Heat Capacity 1.259 J/g-°C
0.3009 BTU/lb-°F
ASTM E-1269-05
Haysite SDL® H261 Polyester, Static Dissipative
H261 is an advanced composite that combines high temperature resistant and high strength characteristics with static dissipative properties for use as wave and reflow solder pallets. SDL Grade H261..