Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 1.50 J/g-°C | 0.359 BTU/lb-°F | IEC 1006 |
Polycasa XT 620 PMMA QUINN XT sheets have good optical properties and a brilliant surface. QUINN XT sheets offer excellent transparency, good mechanical properties, are UV resistant, have very good weathering and ageing.. |
|||
Specific Heat Capacity | 1.50 J/g-°C | 0.359 BTU/lb-°F | |
Plaskolite West Optix® PL-25 Acrylic Resin Extrusion grade pellets. Highest molecular weight and heat resistance of Optix® line. |
|||
Specific Heat Capacity | 1.50 J/g-°C | 0.359 BTU/lb-°F | DSC |
Solvay Specialty Polymers Hylar® MP10 PVDF Polyvinylidene Fluoride
(discontinued **) Data provided by the manufacturer.Hylar® polymers have the characteristic stability of fluoropolymers combined with a unique polarity that influences its solubility and electrical properties. In a.. |
|||
Specific Heat Capacity | 1.50 - 1.60 J/g-°C | 0.359 - 0.382 BTU/lb-°F | DSC |
Wacker Silicones Geniomer® 140 Silicone TPE SLM TPSE 140 is a silicone copolymer containing over 90% siloxane. Geniomer® is a two phase block copolymer made up of a soft polydimethylsiloxane (PDSM) phase and a hard aliphatic isocyanate phas.. |
|||
Specific Heat Capacity | 1.50 J/g-°C | 0.359 BTU/lb-°F | |
Hippe PBT GF 30 Polybutylene Terephthalate 30% Glass fiber Reinforced PBT GF is a highly versatile, semi-crystalline structural thermoplastic reinforced with 30% glass fiber, with very high rigidity and strength characteristics and excellent electrical insulation prop.. |
|||
Specific Heat Capacity | 1.50 J/g-°C | 0.359 BTU/lb-°F | Melt; IEC 1006 |
BASF Ultradur B 2550 PBT Ultradur B2550 is an unfilled, very free-flowing grade for coating paper and board with high heat resistance, for example for packaging of frozen goods and ready-prepared meals. Also suitable for in.. |
|||
Specific Heat Capacity | 1.50 J/g-°C | 0.359 BTU/lb-°F | |
BASF Ultramid® B3EG5 25% Glass Filled PA6 (Dry) Description: 25% glass-fiber reinforced injection-molding grade for industrial articles and electrical insulating partsInformation provided by BASF |
|||
Specific Heat Capacity | 1.50 J/g-°C | 0.359 BTU/lb-°F | |
BASF Ultramid® B3EG6 BK00564 30% Glass Filled PA6 (Dry) Ultramid B3EG6 BK00564 is a 30% glass fiber reinforced, pigmented black injection molding PA6 grade. It conforms to FDA requirements of 21 CFR 177.1500. |
|||
Specific Heat Capacity | 1.50 J/g-°C | 0.359 BTU/lb-°F | |
BASF Ultramid® B3L PA6 (Dry) Ultramid B3L is an impact-modified, easy flowing injection molding PA6 grade for fast processing. |
|||
Specific Heat Capacity | 1.50 J/g-°C | 0.359 BTU/lb-°F | |
BASF Ultramid® A3EG6 30% Glass Filled PA66 (Dry) Ultramid A3EG6 is a 30% glass fiber reinforced injection molding PA66 grade for machinery components and housings of high stiffness and dimensional stability. |
|||
Specific Heat Capacity | 1.50 J/g-°C | 0.359 BTU/lb-°F | |
BASF Ultramid® A3EG7 35% Glass Filled PA66 (Conditioned) Ultramid A3EG6 is a 35% glass fiber reinforced injection molding PA66 grade for machinery components and housings of high stiffness and dimensional stability. |
|||
Specific Heat Capacity | 1.50 J/g-°C | 0.359 BTU/lb-°F | |
BASF Ultramid® B3EG5 25% Glass Filled PA6 (Conditioned) Description: 25% glass-fiber reinforced injection-molding grade for industrial articles and electrical insulating partsInformation provided by BASF |
|||
Specific Heat Capacity | 1.50 J/g-°C | 0.359 BTU/lb-°F | |
BASF Ultramid® B3WG6 BK00564 30% Glass Filled PA6 (Conditioned) Ultramid B3WG6 BK00564 is a 30% glass fiber reinforced, pigmented black, heat stabilized injection molding PA6 grade. |
|||
Specific Heat Capacity | 1.50 - 1.60 J/g-°C | 0.359 - 0.382 BTU/lb-°F | DSC |
Wacker Silicones Geniomer® 80 Silicone TPE SLM TPSE 80 is a silicone copolymer containing over 90% siloxane. Geniomer® is a two phase block copolymer made up of a soft polydimethylsiloxane (PDSM) phase and a hard aliphatic isocyanate phase.. |
|||
Specific Heat Capacity | 1.50 J/g-°C | 0.359 BTU/lb-°F | IEC 1006 |
BASF Ultradur® B 4300 GM42 20/10% Glass/Mineral Filled PBT Description: Is a PBT-HI, mixed glass-fiber-reinforced and mineral-reinforced injection-molding grade with good surface quality and rigidity, and with low warpage for parts such as housings and PCBs.. |
|||
Specific Heat Capacity | 1.50 J/g-°C | 0.359 BTU/lb-°F | IEC 1006 |
BASF Ultradur® B 4500 BK 00110 PBT Information provided by BASF |
|||
Specific Heat Capacity | 1.50 J/g-°C | 0.359 BTU/lb-°F | |
BASF Ultramid® B3L PA6 (Conditioned) Ultramid B3L is an impact-modified, easy flowing injection molding PA6 grade for fast processing. |
|||
Specific Heat Capacity | 1.50 - 1.60 J/g-°C | 0.359 - 0.382 BTU/lb-°F | DSC |
Wacker Silicones Geniomer® 60 Silicone TPE SLM TPSE 60 is a silicone copolymer containing over 90% siloxane. Geniomer® is a two phase block copolymer made up of a soft polydimethylsiloxane (PDSM) phase and a hard aliphatic isocyanate phase.. |
|||
Specific Heat Capacity | 1.50 J/g-°C | 0.359 BTU/lb-°F | IEC 1006 |
BASF Ultradur B 4300 G6 30% Glass Filled PBT Ultradur B4300 G6 is an easy flowing injection molding PBT with 30% glass fiber reinforcement for rigid, tough, and dimensionally stable parts.Applications: Program switches, thermostat parts, small.. |
|||
Specific Heat Capacity | 1.50 J/g-°C | 0.359 BTU/lb-°F | |
BASF Ultramid® B3WG6 BK00564 30% Glass Filled PA6 (Dry) Ultramid B3WG6 BK00564 is a 30% glass fiber reinforced, pigmented black, heat stabilized injection molding PA6 grade. |