Thermal Properties Metric English Comments
Specific Heat Capacity 1.40 - 1.60 J/g-°C
0.335 - 0.382 BTU/lb-°F
Average value: 1.49 J/g-°C Grade Count:3
Overview of materials for Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled". Specific grades with glass content between 45..
Specific Heat Capacity 1.60 - 1.60 J/g-°C

@Temperature 100 - 100 °C
0.382 - 0.382 BTU/lb-°F

@Temperature 212 - 212 °F
Average value: 1.60 J/g-°C Grade Count:21
Overview of materials for Polyvinylidinefluoride (PVDF), Molded/Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polyvinylidinefluoride (PVDF), Molded/Extruded". Each property range of values reported is minimum and m..
Specific Heat Capacity 1.50 - 1.60 J/g-°C
0.359 - 0.382 BTU/lb-°F
Average value: 1.58 J/g-°C Grade Count:6
Overview of materials for Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled". Each property range of values reported is mini..
Specific Heat Capacity 1.50 - 1.60 J/g-°C
0.359 - 0.382 BTU/lb-°F
DSC
Wacker Silicones Geniomer® 140 Silicone TPE
SLM TPSE 140 is a silicone copolymer containing over 90% siloxane. Geniomer® is a two phase block copolymer made up of a soft polydimethylsiloxane (PDSM) phase and a hard aliphatic isocyanate phas..
Specific Heat Capacity 1.50 - 1.60 J/g-°C
0.359 - 0.382 BTU/lb-°F
DSC
Wacker Silicones Geniomer® 200 Silicone TPE Elastomer
SLM TPSE 200 is a silicone copolymer containing over 90% siloxane. Geniomer® is a two phase block copolymer made up of a soft polydimethylsiloxane (PDSM) phase and a hard aliphatic isocyanate phas..
Specific Heat Capacity 1.50 - 1.60 J/g-°C
0.359 - 0.382 BTU/lb-°F
DSC
Wacker Silicones Geniomer® 80 Silicone TPE
SLM TPSE 80 is a silicone copolymer containing over 90% siloxane. Geniomer® is a two phase block copolymer made up of a soft polydimethylsiloxane (PDSM) phase and a hard aliphatic isocyanate phase..
Specific Heat Capacity 1.50 - 1.60 J/g-°C
0.359 - 0.382 BTU/lb-°F
DSC
Wacker Silicones Geniomer® 60 Silicone TPE
SLM TPSE 60 is a silicone copolymer containing over 90% siloxane. Geniomer® is a two phase block copolymer made up of a soft polydimethylsiloxane (PDSM) phase and a hard aliphatic isocyanate phase..