Polymer Property : Specific Heat Capacity = 1.59 J/g-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Specific Heat Capacity 1.17 - 1.59 J/g-°C
0.280 - 0.380 BTU/lb-°F
Saint-Gobain Norton® PVDF Fluoropolymer Film
Features/Benefits:Excellent weatherabilityHigh dielectric strengthExcellent chemical and abrasion resistanceThermoformableProduct available in widths up to 60"Product available with thicknesses from..