Thermal Properties Metric English Comments
DSC Induction Temperature 250 °C
482 °F
LyondellBasell Alathon® L4904 High Density Polyethylene, Pipe and Sheet Extrusion Grade
Alathon L4904 is a bimodal, high molecular weight, high density polyethylene resin with excellent processability characteristics that meet the high performance requirements of demanding pressure pip..
DSC Induction Temperature >= 250 °C
>= 482 °F
ASTM D3350
LyondellBasell Alathon® L5008 High Density Polyethylene
ApplicationsALATHON L 5008 is a high molecular weight high density polyethylene copolymer resin with broad and bimodal molecular weight distribution.Regulatory StatusWhen L 5008 is compounded with a..
DSC Induction Temperature 250 °C
482 °F
LyondellBasell Alathon® L5008HP High Density Polyethylene, Pressure Pipe Extrusion Grade
ALATHON L5008HP is a bimodal, high molecular weight, high density polyethylene resin with excellent processability designed to meet the high performance requirements of pressure pipe applications in..
DSC Induction Temperature 250 °C
482 °F
Average value: 250 °C Grade Count:3
Overview of materials for High Density Polyethylene (HDPE), Pipe Grade
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Pipe Grade". Each property range of values reported is minimum and max..