Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | -13.0 °C | 8.60 °F | |
Asahi Glass AFLAS® MZ TFE/P/VdF Fluoroelastomer AFLAS® MZ is a terpolymer composed of tetrafluoroethylene, propylene and vinylidene fluoride. AFLAS® MZ offers a good balance of chemical resistance and improved low temperature performance and is.. |