Polymer Property : Glass Transition Temp, Tg = 8.60 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -13.0 °C
8.60 °F
Asahi Glass AFLAS® MZ TFE/P/VdF Fluoroelastomer
AFLAS® MZ is a terpolymer composed of tetrafluoroethylene, propylene and vinylidene fluoride. AFLAS® MZ offers a good balance of chemical resistance and improved low temperature performance and is..