Polymer Property : Glass Transition Temp, Tg = -21.0 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -29.4 °C
-21.0 °F
ASTM D1329
Seals Eastern 5400 Nitrile Rubber
General purpose NitrileInformation provided by Seals Eastern, Inc.
Glass Transition Temp, Tg -29.4 °C
-21.0 °F
ASTM D1329
Seals Eastern 5401 Nitrile Rubber
General purpose NitrileInformation provided by Seals Eastern, Inc.
Glass Transition Temp, Tg -29.4 °C
-21.0 °F
ASTM D1329
Seals Eastern 5407 Nitrile Rubber
General purpose Nitrile; Peroxide curedInformation provided by Seals Eastern, Inc.
Glass Transition Temp, Tg -29.4 °C
-21.0 °F
ASTM D1329
Seals Eastern 5433 Nitrile Rubber
General purpose Nitrile; Low water swellInformation provided by Seals Eastern, Inc.
Glass Transition Temp, Tg -29.4 °C
-21.0 °F
ASTM D1329
Seals Eastern 5484 Nitrile Rubber
Low temperature service NitrileInformation provided by Seals Eastern, Inc.
Glass Transition Temp, Tg -29.4 °C
-21.0 °F
ASTM D1329
Seals Eastern 5403 Nitrile Rubber
General purpose NitrileInformation provided by Seals Eastern, Inc.
Glass Transition Temp, Tg -29.4 °C
-21.0 °F
ASTM D1329
Seals Eastern 5404 Nitrile Rubber
General purpose NitrileInformation provided by Seals Eastern, Inc.