Glass Transition Temp, Tg -37.8 °C
-36.0 °F
DSC, 10ºC/min; DIN 51.007
Lubrizol Advanced Materials PEARLTHANE® 11T92EM Thermoplastic Polyurethane Elastomer
PEARLTHANE® 11T92EM is a polyester based TPU, supplied in form of translucent, colourless or slightly yellowish pellets, combining hardness with excellent mechanical properties. It can be extrude..
Glass Transition Temp, Tg -37.8 °C
-36.0 °F
DSC
Lubrizol Estane® ZHF 80AT3 Thermoplastic Polyurethane, Flame Retardant
Type: Estane® ZHF 80AT3 NAT 022 is an 80A non halogen, flame retardant, aromatic polyether-based thermoplastic polyurethane (TPU).Appearance: Transparent spherical pelletsFeatures: Zero halogenUses..