Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lubrizol Estane® ZHF 80AT3 Thermoplastic Polyurethane, Flame Retardant

Category Polymer , Thermoplastic , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyether Grade
Manufacturer Lubrizol (former Noveon)
Trade Name ESTANE®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol Estane® ZHF 80AT3 Thermoplastic Polyurethane, Flame Retardant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Type: Estane® ZHF 80AT3 NAT 022 is an 80A non halogen, flame retardant, aromatic polyether-based thermoplastic polyurethane (TPU).Appearance: Transparent spherical pelletsFeatures: Zero halogenUses: Wire and CableAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformation Provided by The Lubrizol Corporation
Physical Properties Metric English Comments
Specific Gravity 1.12 g/cc
1.12 g/cc
ASTM D792
Maximum Moisture Content 0.050
0.050
Mechanical Properties Metric English Comments
Hardness, Shore A 80
80
ASTM D2240
Tensile Strength, Ultimate 46.0 MPa
6670 psi
ASTM D412
Elongation at Break 600 %
600 %
ASTM D412
Taber Abrasion, mg/1000 Cycles 340

@Load 1.00 kg
340

@Load 2.20 lb
H-18 wheel; ASTM D3389
Compression Set 20 %
20 %
ASTM D395
Tensile Set 20 %
20 %
ASTM D412
Thermal Properties Metric English Comments
Vicat Softening Point 90.0 °C
194 °F
ASTM D1525
Glass Transition Temp, Tg -37.8 °C
-36.0 °F
DSC
Flammability, UL94 V-2

@Thickness 1.91 mm
V-2

@Thickness 0.0750 in
Component Elements Properties Metric English Comments
Loss on Ignition(%) 25 %
25 %
Processing Properties Metric English Comments
Zone 1 185 °C
365 °F
Extrusion
Zone 2 185 °C
365 °F
Extrusion
Zone 3 190 °C
374 °F
Extrusion
Zone 4 185 °C
365 °F
Extrusion
Adapter Temperature 185 °C
365 °F
5, Extrusion
Die Temperature 180 °C
356 °F
6, Extrusion
180 °C
356 °F
7, tip, Extrusion
Drying Temperature 100 °C
212 °F
Dry Time 3.00 hour
3.00 hour
Dew Point -40.0 °C
-40.0 °F