Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Glass Transition Temp, Tg = -39.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -39.0 °C
-38.2 °F
ASTM D4065
Solvay Specialty Polymers Solef® 460/461 Polyvinylidene Fluoride (PVDF)  (Unverified Data**)
Solef® 460/461 PVDF homopolymer has high melt viscosity and is typically processed by extrusion.Information provided by Solvay Specialty Polymers.
Glass Transition Temp, Tg -39.0 °C
-38.2 °F
Midpoint; ASTM E 1269
Huntsman IROGRAN® PS455-203 TPU-Polyester
Polyester-based grades with a broad processing window ideally suited for cast, flat die and flown film lines.Information provided by Alliance Polymers
Glass Transition Temp, Tg -39.0 °C
-38.2 °F
ASTM E1356
Solvay Specialty Polymers Solef® 460/461 Polyvinylidene Fluoride (PVDF)
Solef® 460/461 PVDF homopolymer has high melt viscosity and is typically processed by extrusion.Features: High Viscosity; HomopolymerAdditional Properties: Crystallization Heat - ASTM D3418 46.0 ..
Glass Transition Temp, Tg -39.0 °C
-38.2 °F
DSC
Lubrizol Estane® ETE 55DS3 Thermoplastic Polyurethane, Easy-to-Extrude
Type: Estane® ETE 55DS3 is a 55D aromatic polyester-based thermoplastic polyurethane (TPU).Features: Hard TPU with wide extrusion processing window and melt stability, low temperature flexibility, ..
Glass Transition Temp, Tg -39.0 °C
-38.2 °F
DSC
Lubrizol Estane® 5712 Thermoplastic Polyurethane
Type: Estane® 5712 is a Polyester thermoplastic polyurethane (TPU).Feature: It has the highest peel and green strengths and shortest open-tack time of any Estane TPU resin used in adhesives. Suppl..
Glass Transition Temp, Tg -39.0 °C
-38.2 °F
Lubrizol Estane® 2102-75A Thermoplastic Polyurethane Elastomer
Formerly PellethaneFeature: Memory, elasticity and impact modificationAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane prod..
Copyright © lookpolymers.com All Rights Reserved