Polymer Property : Glass Transition Temp, Tg = -65.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -65.0 °C
-85.0 °F
ASTM D1329
Seals Eastern 5053 Ethylene-Propylene Rubber
General service EPDM.Information provided by Seals Eastern, Inc.
Glass Transition Temp, Tg -65.0 °C
-85.0 °F
ASTM D3418
DSM Biomedical BioSpan® SPU Segmented Polyether Polyurethane (SPU)
The flex life exhibited by BioSpan® SPU enables good performance in many different types of medical devices. This elastomeric polymer has shown the ability to withstand millions of flex cycles.The ..
Glass Transition Temp, Tg -65.0 °C
-85.0 °F
10°C/min
Arkema Group Pebax® 2533 SN 01 Polyether Block Amide (PEBA) (Dry)
POLYETHER BLOCK AMIDE (PEBA) hardness 25 shore D Non plasticized flexible Polyamide Outstanding mechanical properties at low temperature (-40°C) Applications: molded parts for sport goods (softness..
Glass Transition Temp, Tg -65.0 °C
-85.0 °F
10°C/min
Arkema Group Pebax® 3533 SN 01 Polyether Block Amide (PEBA) (Dry)
POLYETHER BLOCK AMIDE (PEBA) hardness 35 shore D Non plasticized flexible Polyamide Outstanding mechanical properties at low temperature (-40°C) Applications: molded parts for sport goods (softness..
Glass Transition Temp, Tg -65.0 °C
-85.0 °F
10°C/min
Arkema Group Pebax® 4033 SN 01 Polyether Block Amide (PEBA) (Dry)
POLYETHER BLOCK AMIDE (PEBA) hardness 40 shore D Non plasticized flexible Polyamide Outstanding mechanical properties at low temperature (-40°C) Applications: molded parts for sport goods (softness..
Glass Transition Temp, Tg -65.0 °C
-85.0 °F
10°C/min
Arkema Group Pebax® MX 1059 Polyether Block Amide (PEBA) (Dry)
POLYETHER BLOCK AMIDE (PEBA) Hardness 35 shore D Good resistance to oils. Applications: Automotive, cable...ISO data provided by the manufacturer, Arkema.
Glass Transition Temp, Tg -65.0 °C
-85.0 °F
Cured property; JMTP P200
Aptek 2100-A/B Urethane Encapsulant and/or Potting Compound
General purpose encapsulant and potting compound. Outstanding hydrolytic stability. Excellent adhesion to components/circuit boards. Low modulus, low stress. Field proven for military and space appl..
Glass Transition Temp, Tg -65.0 °C
-85.0 °F
Cured property; ASTM E831-86
Aptek 7503LM-PMF UV Urethane Conformal Coating
UV-cured, low modulus, shadow cures under components. Excellent adhesion without primer. Repairable. Qualified to MIL-I-46058C, types UR and AR. Castable version – UVIKOTE 7504 LM-PMF.Information p..
Glass Transition Temp, Tg -65.0 °C
-85.0 °F
Cured property; ASTM E831-86
Aptek 7504LM-PMF UV Urethane Coating/Encapsulant
UV-cured,100% solids version of UVIKOTE 7503 LM-PMF. Castable/brushable viscosity for higher coating build-up. QPL listed on MIL-I-46058C, types UR an AR.Information provided by Aptek Laboratories, ..
Glass Transition Temp, Tg -65.0 - -50.0 °C
-85.0 - -58.0 °F
Average value: -58.6 °C Grade Count:7
Overview of materials for Polyether Block Amide (PEBA)
This property data is a summary of similar materials in the MatWeb database for the category "Polyether Block Amide (PEBA)". Each property range of values reported is minimum and maximum values of a..