Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -70.0 °C
-94.0 °F
Natural Rubber, Not Vulcanized (NR, IR, Polyisoprene)
Natural rubber is polyisoprene. Chemical and environmental resistance and mechanical properties are improved through crosslinking (vulcanizing), usually through treatment with sulfur.Natural rubber..
Glass Transition Temp, Tg -70.0 °C
-94.0 °F
Styron XZ 92027.00 Carboxylated Butadiene Acrylate
Performance Features: General purpose paper removable PSA, low adhesive transfer to paper and polyolefin substrates Applications: PSAEuropeInformation provided by Styron
Glass Transition Temp, Tg -70.0 °C
-94.0 °F
DSC
Lubrizol Estane® 58123 Thermoplastic Polyurethane
Features: High moisture vapor transmission with low water swell and excellent low temperature and elasticity properties.Uses: Blown and flat die/cast film extrusion, injection molding and cable jack..
Glass Transition Temp, Tg -70.0 °C
-94.0 °F
DSC
Lubrizol Estane® MVT 70AT3 Thermoplastic Polyurethane, Moisture Vapor Transmission
Type: Estane® MVT 70AT3 is an aromatic polyether-based thermoplastic polyurethane (TPU).Features: High moisture vapor transmission with low water swell. Excellent low temperature properties and el..
Glass Transition Temp, Tg -70.0 °C
-94.0 °F
ASTM D3418
DSM Biomedical BioSpan® F SPU Segmented Polyether Polyurethane (SPU)
The flex life exhibited by BioSpan® SPU enables good performance in many different types of medical devices. This elastomeric polymer has shown the ability to withstand millions of flex cycles.The ..
Glass Transition Temp, Tg -70.0 °C
-94.0 °F
3M Scotchcast™ 2104 Electrical Insulating Resin
Scotchcast 2104 Electrical Insulating Resin is a hard, two-part, polyurethane resin encapsulant designed especially for permanent splice protection. 2104 is formulated for virtually every electrical..
Glass Transition Temp, Tg -70.0 °C
-94.0 °F
Cured property; JMTP 200
Aptek 2100-A7C/B Low modulus urethane staking compound
APTEK 2100-A7C/B is a thixotropic, two component, electrically insulating, low modulus urethane system designed for the staking of electrical/electronic components to printed circuit boards. Althoug..
Glass Transition Temp, Tg -70.0 °C
-94.0 °F
Cured property; JMTP P-200
Aptek 2205 A/B Low modulus urethane stacking compound
APTEK 2205-A/B is a thixotropic, two component, electrically insulating, low modulus urethane system designed for the staking of electrical/electronic components to printed circuit boards. Although..
Glass Transition Temp, Tg <= -70.0 °C
<= -94.0 °F
ASTM D746
Ashley Polymers Ashlene® 935-40M Nylon 11
A rotational molding grade Nylon 11 with a 40-50 mesh.Data provided by the manufacturer
Glass Transition Temp, Tg -70.0 °C
-94.0 °F
Cured property; JMTP P-100
Aptek DAT-A-THERM 1000 Electrically insulating urethane film
DAT-A-THERM 1000 is a tough, flexible, void free, electrically insulating urethane film designed to fill air gaps and dissipate heat between devices and substrates. DAT-A-THERM 1000 film is a 100% s..