Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 90.0 - 111 °C | 194 - 232 °F | Average value: 103 °C Grade Count:9 |
Overview of materials for Cellulose Acetate Propionate, Molded This property data is a summary of similar materials in the MatWeb database for the category "Cellulose Acetate Propionate, Molded". Each property range of values reported is minimum and maximum val.. |