Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 90.0 - 140 °C | 194 - 284 °F | Average value: 123 °C Grade Count:3 |
Overview of materials for Thermoset Polyurethane, Liquid, Quartz Filled This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Liquid, Quartz Filled". Each property range of values reported is minimum and ma.. |