Polymer Property : Glass Transition Temp, Tg = 18.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 18.0 °C
64.4 °F
Styron XZ 94714.01 Carboxylated SB
Performance Features: Anti-corrosion primerApplications: Fiber Binding, Glass Fiber Binding, Nonwovens and Thermo MoldableEuropeInformation provided by Styron
Glass Transition Temp, Tg 18.0 °C
64.4 °F
Ultimate Tg
Tra-Con Tra-Bond 216C03 Flexible Plastic Bonder
TRA-BOND 216C03 is a flexible thixotropic bonding adhesive designed for bonding all types of plastics including nylon, PVC, polyethylene, acrylic, lexan, polypropylene, kapton or almost any thermopl..
Glass Transition Temp, Tg 18.0 °C
64.4 °F
Ultimate Tg
Tra-Con Tra-Bond 216C05
Information provided by Tra-Con Inc.